NAC590.010. Adoption by reference of specifications for antifreeze; additional specifications.  


Latest version.
  • Except as otherwise provided in NAC 590.030:

         1. The specifications for antifreeze based on ethylene glycol and the specifications for antifreeze based on propylene glycol contained in Volume 15.05, “Engine Coolants,” of the 2001 Annual Book of ASTM Standards, ASTM designation D3306-00a, are hereby adopted by reference.

         2. The chemical and physical properties of any antifreeze other than those classified in subsection 1 must be:

         Water, mass %.............................................

                                                                5 max

         Specific gravity 60°F/60°F..........................     

                                                      1.11 to 1.15

         pH (33% by volume) 7.5 to 11...................

                                                           7.5 to 11

         Equilibrium boiling point............................

                                                         300°F min

         Freezing point, 50% by volume..................

                                                         -34°F max

         Foaming test

              Increase in volume at 5 minutes.............

                                                       150 ml max

         Break time...................................................

                                                          5 sec max

         3. In addition to the properties listed in subsection 2, any antifreeze other than those classified in subsection 1 must meet the following specifications for corrosion (loss of weight per specimen):

         Copper.........................................................

                                                        10 mg max

         Solder..........................................................

                                                        20 mg max

         Brass............................................................

                                                        10 mg max

         Steel.............................................................

                                                        10 mg max

         Cast iron......................................................

                                                        10 mg max

         Aluminum....................................................

                                                        30 mg max

         4. Any other test method may be used if the State Sealer of Consumer Equitability determines that another method produces results equivalent to the results of the specified method. A method approved by ASTM International that has not yet been published shall be deemed to meet the appropriate criteria.

     [Dep’t of Agriculture, No. 90.30, eff. 5-1-73]—(NAC A 3-17-86; 8-9-94; A by St. Sealer of Weights & Measures by R149-98, 12-14-98; R200-01, 5-31-2002)